Abstract
This chapter addresses some of the challenges involved in materials selection, providing context for much of the information presented in the book. It describes a typical four-step design scenario, noting material-related considerations and information needs. It explains how design decisions are complicated by the interconnected nature of material properties, design geometry, and manufacturing requirements and effects. The chapter also assesses the design impact of several materials and discusses codes, standards, and specifications.
The Materials Selection Process, Metallurgy for the Non-Metallurgist, 2nd ed., Edited By Arthur C. Reardon, ASM International, 2011, p 407–428, https://doi.org/10.31399/asm.tb.mnm2.t53060407