Chapter 16: The Durability of Metals and Alloys
-
Published:2011
Abstract
Durability is a generic term used to describe the performance of a material or a component made from that material in a given application. In order to be durable, a material must resist failure by wear, corrosion, fracture, fatigue, deformation, and exposure to a range of service temperatures. This chapter covers several types of component and material failure associated with wear, temperature effects, and crack growth. It examines temperature-induced, brittle, ductile, and fatigue failures as well as failures due to abrasive, erosive, adhesive, and fretting wear and cavitation fatigue. It also discusses preventative measures.
Sign in
ASM members
Member Sign InThe Durability of Metals and Alloys, Metallurgy for the Non-Metallurgist, 2nd ed., Edited By Arthur C. Reardon, ASM International, 2011, p 385–405, https://doi.org/10.31399/asm.tb.mnm2.t53060385
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.