Metallurgy for the Non-Metallurgist (Second Edition)
Chapter 9: Heat Treatment of Steel
-
Published:2011
Abstract
This chapter discusses the types, methods, and advantages of heat treating procedures, including annealing, normalizing, tempering, and case hardening. It describes the iron-carbon system, the formation of equilibrium and metastable phases, and the effect of alloy elements on hardenability and tempering response. It discusses the significance of critical temperatures, the use of transformation diagrams, and types of annealing treatments. It also provides information on heat treating furnaces, the effect of heating rate on transformation temperatures, quench and temper procedures, and the use of cold treating.
Heat Treatment of Steel, Metallurgy for the Non-Metallurgist, 2nd ed., Edited By Arthur C. Reardon, ASM International, 2011, p 197–246, https://doi.org/10.31399/asm.tb.mnm2.t53060197
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.