Metallurgy for the Non-Metallurgist (Second Edition)
Chapter 5: Modern Alloy Production
-
Published:2011
Abstract
This chapter describes the processes involved in alloy production, including melting, casting, solidification, and fabrication. It discusses the effects of alloying on solidification, the formation of solidification structures, supercooling, nucleation, and grain growth. It describes the design and operation of melting furnaces as well as melting practices and the role of fluxing. It also discusses casting methods, nonferrous casting alloys, and atomization processes used to make metal powders.
Sign in
ASM members
Member Sign InModern Alloy Production, Metallurgy for the Non-Metallurgist, 2nd ed., Edited By Arthur C. Reardon, ASM International, 2011, p 85–115, https://doi.org/10.31399/asm.tb.mnm2.t53060085