This chapter contains a corrosion rate conversion table and a figure that shows the relationships among some of the units commonly used for corrosion rates of metals.
Topics
Atmospheric corrosion,
Gaseous corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Galvanic corrosion,
Weld corrosion,
Stray current corrosion,
Stress corrosion cracking,
Hydrogen embrittlement,
Carbon steel,
Stainless steel,
Corrosion inhibitors,
Chemical and petrochemical processing equipment,
Oil and gas refining equipment,
Nonferrous metals and alloys,
Corrosion,
Ferrous metals and alloys
You do not currently have access to this chapter.
Citation
Corrosion Rate Conversion, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 396, https://doi.org/10.31399/asm.tb.cpi2.t55030396
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.
Related Book Content
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Conversion Table
Mechanics and Mechanisms of Fracture An Introduction
Factors for Calculating Di for Steels as Given in ASTM Standard A255-67
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Temperature Conversions
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Basic Concepts Important to Corrosion
Corrosion: Understanding the Basics
Corrosion Rate Conversion
Corrosion: Materials
Corrosion Data
Titanium: A Technical Guide (Second Edition)
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Attack Polishing Procedures
Metallography Principles and Practice