Corrosion in the Petrochemical Industry (Second Edition)
Abstract
This chapter focuses on various factors to be considered at design stage to minimize corrosion. It begins by providing information on design considerations and general corrosion awareness. This is followed by a description of several factors influencing materials-component failure. Details on design and materials selection, which assist in controlling corrosion, are then provided. The chapter ends with a discussion on the design factors that influence corrosion.
Sign in
ASM members
Member Sign InDesigning to Minimize Corrosion, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 235–244, https://doi.org/10.31399/asm.tb.cpi2.t55030235