Corrosion Resistance of Stainless Steels and Nickel Alloys[1]
-
Published:2015
Page range:
176 - 179
Abstract
Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This chapter examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on the corrosion resistance of these alloys. Some categories of corrosion covered are pitting, crevice, intergranular, stress-corrosion cracking, general, and high-temperature corrosion.
You do not currently have access to this chapter.
Citation
Corrosion Resistance of Stainless Steels and Nickel Alloys, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 176–179, https://doi.org/10.31399/asm.tb.cpi2.t55030176
Download citation file:
Related Book Content
Corrosion of Austenitic Stainless Steel Weldments
Corrosion of Weldments
Duplex Stainless Steels
Stainless Steels for Design Engineers
Corrosion of Wrought Stainless Steels
Corrosion: Materials
Localized Corrosion
Fundamentals of Electrochemical Corrosion
Monitoring and Testing of Weld Corrosion
Corrosion of Weldments
Materials Selection for Corrosion Control
Corrosion in the Petrochemical Industry (Second Edition)
Environmentally-Induced Failures
Fatigue and Fracture Understanding the Basics
Failure of Non-Magnetic Retaining Ring in a High-Speed Generator Rotor
Handbook of Case Histories in Failure Analysis
Fractured Lock Ring of Drum
ASM Failure Analysis Case Histories: Mechanical and Machine Components
Corrosion of Titanium and Titanium Alloys
Corrosion: Materials