This chapter addresses the general effects of composition, mechanical treatment, surface treatment, processing, and fabrication operations on the corrosion resistance of aluminum and its alloys. Different types of surface treatments covered include claddings, anodizing, and conversion coatings. The processing steps that can have relatively significant impact on corrosion resistance are homogenization, rolling, extrusion, quenching, aging, and annealing.