Abstract
This chapter focuses on resistance characteristics and methods of protecting different forms of high-temperature gaseous corrosion, namely high-temperature oxidation, sulfidation, carburization, hydrogen effects, and hot corrosion.
You do not currently have access to this chapter.
Citation
High-Temperature Gaseous Corrosion, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 25–32, https://doi.org/10.31399/asm.tb.cpi2.t55030025
Download citation file:
Related Book Content
High-Temperature Gaseous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Gaseous Corrosion Mechanisms
Corrosion: Fundamentals, Testing, and Protection
Corrosion in High-Temperature Environments
Corrosion: Environments and Industries
High-Temperature Corrosion-Related Failures
Failure Analysis and Prevention
Corrosion of Intermetallics
Corrosion: Materials
Corrosion of Metal Processing Equipment
Corrosion: Environments and Industries
Corrosion of Cast Stainless Steels
Corrosion: Materials
Corrosion and Protection of Superalloys
Superalloys: A Technical Guide (Second Edition)
Hot Corrosion in Gas Turbines
High-Temperature Corrosion and Materials Applications
Introduction to Surface Engineering for Corrosion and Wear Resistance
Surface Engineering for Corrosion and Wear Resistance