This article depicts typical fractographic features for a number of different composite materials, covering interlaminar and translaminar fracture characteristics in composite materials.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Fractography of Composites, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 417–429, https://doi.org/10.31399/asm.tb.cfap.t69780417
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Fractography
Composites
Fatigue Fracture Appearances
Failure Analysis and Prevention
Failure of a Throttle End Fitting in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Glossary of Filament-Winding Terms
Composite Filament Winding
Repair
Structural Composite Materials
Examination Methods
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Bolts in a Radar Antenna System Reflector Joint
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Main Wheel Bearing Housing Flange in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Stabilizer Link Rod in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories