Characterization and Failure Analysis of Plastics
Edited by
ASM International
ISBN electronic:
978-1-62708-281-5
Publication date:
2003
Abstract
This article discusses the molecular mechanism, environmental criteria, and material optimization of environmental stress crazing (ESC) in glassy thermoplastics, polyethylenes, and nylons. In addition, it provides information on various tests used to determine relative susceptibility to ESC, namely constant tensile load testing and constant-strain testing.
You do not currently have access to this chapter.
Citation
Environmental Stress Crazing, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 305–313, https://doi.org/10.31399/asm.tb.cfap.t69780305
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Evaluating Stress-Corrosion Cracking
Corrosion: Fundamentals, Testing, and Protection
Wear Failures of Plastics
Characterization and Failure Analysis of Plastics
Wear Failures of Plastics
Failure Analysis and Prevention