Characterization and Failure Analysis of Plastics
Edited by
ASM International
ISBN electronic:
978-1-62708-281-5
Publication date:
2003
Abstract
This article discusses various factors influencing general polymeric behavior, ductile-brittle transitions, crazing, and the brittle fracture of polymeric materials. The discussion covers the effects of environment on glassy thermoplastic, several parametric descriptions of craze initiation, the kinetics of craze growth, and the effect of crazing on toughness of the plastic. In addition, the article provides information on various tests to determine stress-to-craze value, strain-to-craze value, and fracture toughness of the plastic.
You do not currently have access to this chapter.
Citation
Crazing and Fracture, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 204–210, https://doi.org/10.31399/asm.tb.cfap.t69780204
Download citation file:
Related Book Content
Techniques of Failure Analysis
Understanding How Components Fail (Third Edition)
Plastic Design Methods
Characterization and Failure Analysis of Plastics
Viscoelasticity of Plastics
Characterization and Failure Analysis of Plastics
Ultrasonic Nondestructive Analysis of Plastics
Characterization and Failure Analysis of Plastics
Glossary of Terms—Characterization and Failure Analysis of Plastics
Characterization and Failure Analysis of Plastics
Abbreviations—Characterization and Failure Analysis of Plastics
Characterization and Failure Analysis of Plastics
Failure Analysis of Open End Wrenches Containing Forging Defects
Handbook of Case Histories in Failure Analysis
Solvent-Induced Cracking Failure of Polycarbonate Ophthalmic Lenses
Handbook of Case Histories in Failure Analysis
Tensile Testing of Plastics
Tensile Testing (Second Edition)
Environmental Stress Cracking
Characterization and Failure Analysis of Plastics