Abstract
This article describes the basic approaches to improving the fire resistance of a polymeric material, considers the burning process on a microscale and macroscale, and discusses various test methods for determining the flammability characteristics of polymeric materials. Test methods are classified in two ways: by fire response characteristics and by particular applications of polymeric materials.
You do not currently have access to this chapter.
Citation
Flammability Testing, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 159–163, https://doi.org/10.31399/asm.tb.cfap.t69780159
Download citation file:
Related Book Content
Flammability Testing of Plastics
Characterization and Failure Analysis of Plastics
Flammability Testing of Polymers
Engineered Materials Handbook Desk Edition
Material Jetting of Polymers
Additive Manufacturing Processes
Powder Bed Fusion of Polymers
Additive Manufacturing Processes
Differential Scanning Calorimetry
Materials Characterization (2019 Edition)
Friction and Wear Testing
Characterization and Failure Analysis of Plastics
Introduction
Binder and Polymer Assisted Powder Processing
Glossary
Binder and Polymer Assisted Powder Processing
Fatigue and Fracture of Ceramics and Polymers
Fatigue and Fracture Understanding the Basics
Rheological Testing of Polymers
Characterization and Failure Analysis of Plastics