This chapter is a brief account of the composition, microstructures, heat treatment, deformation mechanisms, mechanical properties, formability, and special attributes of austenitic stainless steels.
You do not currently have access to this chapter.
Citation
Austenitic Stainless Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 151–158, https://doi.org/10.31399/asm.tb.ahsssta.t53700151
Download citation file:
Related Book Content
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Dual-Phase Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Complex-Phase Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Transformation-Induced Plasticity Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Austenitic Stainless Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Steel Fundamentals
Advanced-High Strength Steels Science, Technology, and Applications
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications