Book Chapter
Chapter 9: Twinning-Induced Plasticity Steels
-
Published:2013
Page range:
135 - 149
Abstract
This chapter briefly discusses the characteristics of mechanical twins and stacking faults in close-packed planes. It provides an overview of the composition, microstructures, thermodynamics, processing, deformation mechanism, mechanical properties, formability, and special attributes of twinning-induced plasticity steels.
You do not currently have access to this chapter.
Citation
Twinning-Induced Plasticity Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 135–149, https://doi.org/10.31399/asm.tb.ahsssta.t53700135
Download citation file:
Related Book Content
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Dual-Phase Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Complex-Phase Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Transformation-Induced Plasticity Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Austenitic Stainless Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Steel Fundamentals
Advanced-High Strength Steels Science, Technology, and Applications
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications