Appendix B: Some Additional Microstructural Information
-
Published:2002
Page range:
357 - 363
This appendix provides additional information on superalloy microstructures. It includes several micrographs showing metallographic features mentioned in the text but not illustrated elsewhere in the book. It also discusses carbide reactions that occur during heat treating and demonstrates the use of electron vacancy calculations to estimate the resistance of superalloys to the formation of topologically close-packed phases.
You do not currently have access to this chapter.
Citation
Some Additional Microstructural Information, Superalloys: A Technical Guide, 2nd ed., By Matthew J. Donachie, Stephen J. Donachie, ASM International, 2002, p 357–363, https://doi.org/10.31399/asm.tb.stg2.t61280357
Download citation file:
Related Book Content
Micrograph Gallery
Superalloys Alloying and Performance
Wear Failures of Reinforced Polymers
Characterization and Failure Analysis of Plastics
Phases and Microstructure of Superalloys
Superalloys Alloying and Performance
Introduction
Superalloys Alloying and Performance
Superalloys—Retrospect and Future Prospects
Superalloys: A Technical Guide (Second Edition)
Other Sources
Superalloys: A Technical Guide (Second Edition)
Understanding Superalloy Metallurgy
Superalloys: A Technical Guide (Second Edition)
Overview of Superalloys
Superalloys Alloying and Performance
Selected Superalloy Compositions
Superalloys Alloying and Performance
Superalloys for High Temperatures—a Primer
Superalloys: A Technical Guide (Second Edition)