Abstract
This chapter provides basic materials selection information for iron-nickel-, nickel-, and cobalt-base superalloys. It discusses mechanical and physical properties, the effect of service temperature, and the comparative strengths of wrought and cast product forms. It includes several large data tables along with reference information and a detailed application example based on the design of a gas turbine disk.
You do not currently have access to this chapter.
Citation
Selection of Superalloys, Superalloys: A Technical Guide, 2nd ed., By Matthew J. Donachie, Stephen J. Donachie, ASM International, 2002, p 11–24, https://doi.org/10.31399/asm.tb.stg2.t61280011
Download citation file:
Related Book Content
Superalloys
Metals Handbook Desk Edition (2nd Edition)
333.0 and A333.0 Al-Si-Cu Permanent-Mold Casting Alloy
Properties and Selection of Aluminum Alloys
Structure/Property Relationships in Irons and Steels
Metals Handbook Desk Edition (2nd Edition)
Properties of Metals
Metals Handbook Desk Edition (2nd Edition)
Compositional Effects
Superalloys Alloying and Performance
Structural Alloys
Materials at Low Temperatures
Powder Metallurgy Superalloys
Powder Metallurgy
The Materials Selection Process
Metallurgy for the Non-Metallurgist (Second Edition)
Introduction
Superalloys Alloying and Performance
Superalloys—Retrospect and Future Prospects
Superalloys: A Technical Guide (Second Edition)