Appendix 2: Physical and Mechanical Properties of Select Alloys
-
Published:2008
Abstract
This appendix contains tables listing the physical and mechanical properties of stainless steel engineering alloys. The physical properties covered are density, modulus of elasticity, coefficient of thermal expansion, thermal conductivity, specific heat, and electrical resistivity. The mechanical properties listed include yield strength, tensile strength, elongation and hardness.
Topics
Corrosion,
Stainless steel,
Automobiles and trucks,
Construction and farming equipment,
Casting,
Welding,
Machining,
Forming,
Surface treatment,
Chemical and petrochemical processing equipment,
Offshore and marine equipment,
Oil and gas production equipment,
Pulp and paper processing equipment,
Electrical resistivity,
Elastic modulus,
Hardness,
Elongation,
Tensile strength,
Density,
Thermal conductivity,
Coefficient of thermal expansion,
Specific heat capacity
You do not currently have access to this chapter.
Citation
Physical and Mechanical Properties of Select Alloys, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 279–280, https://doi.org/10.31399/asm.tb.ssde.t52310279
Download citation file:
Related Book Content
Thermal Conductivity and Thermal Diffusivity
Materials at Low Temperatures
Thermomechanical Testing
Metalworking: Bulk Forming
Electromagnetic and Thermal Properties of Materials
Induction Heating and Heat Treatment
Lamina and Laminate Nonmechanical Testing
Composites
Properties of Materials
Elementary Materials Science
Workpiece Materials Database
Metalworking: Bulk Forming
Physical Properties
Steel Castings Handbook (Sixth Edition)
Mechanical Behavior of Materials under Tensile Loads
Tensile Testing (Second Edition)
Failed Missile Launcher Detent Spring
Handbook of Case Histories in Failure Analysis
Theory of Heating by Induction
Practical Induction Heat Treating (Second Edition)