Stainless Steels for Design EngineersAvailable to Purchase
ASM International
ISBN electronic:
978-1-62708-286-0
Publication date:
2008
Book Chapter
Chapter 19: Automotive and Transportation Applications Available to Purchase
-
Published:2008
Page range:
225 - 232
Abstract
This chapter is a detailed account of the applications of stainless steel in automotive and transport systems. The discussion covers exhaust systems, structural components, automotive components, trucks, and rail transport.
You do not currently have access to this chapter.
Citation
Automotive and Transportation Applications, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 225–232, https://doi.org/10.31399/asm.tb.ssde.t52310225
Download citation file:
Related Book Content
Effect of Strain Rate on the Failure Mode of a Rear Axle
Handbook of Case Histories in Failure Analysis
Fatigue Fracture of a Fan Blade
Handbook of Case Histories in Failure Analysis
Fatigue Failure of a 1000 mm (40 in.) Diam Trailer Wheel at the Bolt Holes
Handbook of Case Histories in Failure Analysis
Cracking of a Dump Truck Transmission Housing
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Bacteria-Induced Corrosion of a Stainless Steel Chemical Trailer Barrel
Handbook of Case Histories in Failure Analysis
Broken Exhaust Valve
ASM Failure Analysis Case Histories: Automobiles and Trucks
Failure Analysis of an Automobile Weldment
ASM Failure Analysis Case Histories: Automobiles and Trucks
Use of XRD to Assess Residual Stresses in Steel Springs
ASM Failure Analysis Case Histories: Automobiles and Trucks
Plastics
Gear Materials, Properties, and Manufacture
Distortion Failure of an Automotive Valve Spring
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms