Stainless Steels for Design Engineers
Chapter 12: Melting, Casting, and Hot Processing
-
Published:2008
Abstract
This article discusses the steps in the primary processing of stainless steels: melting, refining, remelting, casting, and hot rolling. It provides information of the major categories of defects in hot rolled stainless steels, namely hot mill defects, inclusion-related defects, and hot ductility-related defects.
Melting, Casting, and Hot Processing, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 155–160, https://doi.org/10.31399/asm.tb.ssde.t52310155