Abstract
This chapter discusses the alloy composition, metallurgy, mechanical behavior, stabilization, texture, anisotropy, high-temperature properties, and corrosion and oxidation resistance of ferritic stainless steels.
You do not currently have access to this chapter.
Citation
Ferritic Stainless Steels, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 109–122, https://doi.org/10.31399/asm.tb.ssde.t52310109
Download citation file:
Related Book Content
Elevated-Temperature Properties of Stainless Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Bainite
Steels: Processing, Structure, and Performance (Second Edition)
Corrosion Resistance of Powder Metallurgy Stainless Steels
Powder Metallurgy
Sintering of Stainless Steels
Powder Metallurgy
Mechanical Behavior of Nonmetallic Materials
Mechanics and Mechanisms of Fracture An Introduction
Effects of Metallurgical Variables on the Corrosion of Stainless Steels
Corrosion in the Petrochemical Industry (Second Edition)
Medical Applications of Stainless Steels
Materials for Medical Devices
Corrosion of Nonferrous Alloy Weldments
Corrosion: Fundamentals, Testing, and Protection
Stainless Steels
Elements of Metallurgy and Engineering Alloys
Forging Design Involving Parting Line and Grain Flow
Metalworking: Bulk Forming