Abstract
This chapter provides information on the structure, design aspects, mechanical properties, forming, machining, and corrosion resistance characteristics of duplex stainless steels. The different types of corrosion covered are general corrosion, pitting corrosion, crevice corrosion, and stress corrosion cracking.
Topics
Corrosion,
Stainless steel,
Automobiles and trucks,
Construction and farming equipment,
Casting,
Welding,
Machining,
Forming,
Surface treatment,
Chemical and petrochemical processing equipment,
Offshore and marine equipment,
Oil and gas production equipment,
Pulp and paper processing equipment,
Crevice corrosion,
Pitting corrosion,
Stress corrosion cracking,
Duplex stainless steel,
Mechanical properties
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Duplex Stainless Steels, Stainless Steels for Design Engineers, By Michael F. McGuire, ASM International, 2008, p 91–107, https://doi.org/10.31399/asm.tb.ssde.t52310091
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Corrosion Resistance of Stainless Steels and Nickel Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Chemical and Process Industry Applications
Stainless Steels for Design Engineers
Nickel and Nickel Alloys
Alloying Understanding the Basics
Corrosion Types
Stainless Steels for Design Engineers
Corrosion Resistance of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Localized Corrosion
Fundamentals of Electrochemical Corrosion
Coping with Corrosion
Metallurgy for the Non-Metallurgist (Second Edition)
Corrosion of Wrought Stainless Steels
Corrosion: Materials
Corrosion of Titanium and Titanium Alloys
Corrosion: Materials
Corrosion of Duplex Stainless Steel Weldments
Corrosion of Weldments