Book Chapter
Appendix III: Conversion Tables Available to Purchase
-
Published:1999
Page range:
459 - 464
Abstract
This appendix includes a temperature conversion table, a table containing equivalent hardness numbers, and a unit conversion table.
You do not currently have access to this chapter.
Citation
Conversion Tables, Light Microscopy of Carbon Steels, By Leonard E. Samuels, ASM International, 1999, p 459–464, https://doi.org/10.31399/asm.tb.lmcs.t66560459
Download citation file:
Related Book Content
Approximate Equivalent Hardness Numbers and Tensile Strengths for Vickers Hardness Numbers for Steel
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Approximate Equivalent Hardness Numbers and Tensile Strengths for Brinell Hardness Numbers for Steel
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Approximate Equivalent Hardness Numbers and Tensile Strengths for Rockwell C and B Hardness Numbers for Steel
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Temperature Conversion Table
Failure Analysis of Heat Treated Steel Components
Metallurgical Investigation of Failed Locked Coil Track Ropes Used in a Mining Conveyor
Handbook of Case Histories in Failure Analysis
Steel Selection for Hardening
Heat Treating of Irons and Steels
Additive Manufacturing of Steels and Stainless Steels
Additive Manufacturing Processes
Tempering of Steels
Steel Heat Treating Fundamentals and Processes
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels