Chapter 3: Phase Transformations Available to Purchase
-
Published:1999
Page range:
29 - 37
Abstract
This chapter describes some of the most essential tools in metallurgy and what they reveal about the structure, composition, and processing requirements of steel. It begins by identifying important details in the constitutional diagram of iron-cementite. It then explains how to read isothermal transformation and continuous-cooling diagrams and how to recognize the effect of various alloying elements.
You do not currently have access to this chapter.
Citation
Noel F. Kennon, Phase Transformations, Light Microscopy of Carbon Steels, By Leonard E. Samuels, ASM International, 1999, p 29–37, https://doi.org/10.31399/asm.tb.lmcs.t66560029
Download citation file:
Related Book Content
Isothermal and Continuous Cooling Transformation Diagrams
Steels: Processing, Structure, and Performance (Second Edition)
Hardenability of Steel
Steel Metallurgy for the Non-Metallurgist
Transformation of Austenite and Quenching of Steel
Practical Heat Treating Basic Principles
Malleable Irons
Alloying Understanding the Basics
Solid Solutions and Phase Transformations
Phase Diagrams Understanding the Basics
Understanding the Metallurgy of Titanium
Titanium: A Technical Guide (Second Edition)
Heat Treating of Alloy Steels
Practical Heat Treating (Second Edition)
A History of Wrought Aluminum Alloys and Applications
Properties and Selection of Aluminum Alloys
Alloying of Beryllium
Beryllium Chemistry and Processing
The Low-Alloy AISI Steels
Steel Metallurgy for the Non-Metallurgist