Appendix: Tables Helpful to the Metallographer
-
Published:2002
Abstract
This appendix is a compilation of tables helpful to metallographers in characterizing irons and steels. The tables include AISI/SAE designations and specific composition ranges for various steels and irons, listings of companies that sell metallographic equipment and supplies, and compositions and usage guidance for etchants, chemical polishing solutions, and coatings.
Tables Helpful to the Metallographer, Metallographer’s Guide: Practices and Procedures for Irons and Steels, By Bruce L. Bramfitt, Arlan O. Benscoter, ASM International, 2002, p 297–319, https://doi.org/10.31399/asm.tb.mgppis.t60400297