Abstract
Steels with martensitic and tempered martensitic microstructures, though sometimes perceived as brittle, exhibit plasticity and ductile fracture behavior under certain conditions. This chapter describes the alloying and tempering conditions that produce a ductile form of martensite in low-carbon steels. It also discusses the effect of tempering temperature on the mechanical behavior and deformation properties of medium-carbon steels.
You do not currently have access to this chapter.
Citation
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 405–437, https://doi.org/10.31399/asm.tb.spsp2.t54410405
Download citation file:
Related Book Content
Deformation, Strengthening, and Fracture of Ferritic Microstructures
Steels: Processing, Structure, and Performance (Second Edition)
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications
Mechanisms and Causes of Failures in Heat Treated Steel Parts
Failure Analysis of Heat Treated Steel Components
Failure Analysis of Weldments
Weld Integrity and Performance
Indentation Hardness Testing of Ceramics
Mechanical Testing and Evaluation
Tempering of Steel
Steels: Processing, Structure, and Performance (Second Edition)
Principles of Shearing, Blanking, and Piercing
Metalworking: Sheet Forming
Analysis of Degradation and Failure Mechanisms that Develop in Hot Forging Die
Handbook of Case Histories in Failure Analysis
Water-Hardening Tool Steels
Tool Steels (Fifth Edition)