This chapter describes heat treatments that produce uniform grain structures, reduce residual stresses, and improve ductility and machinability. It also discusses spheroidizing treatments that improve strength and toughness by promoting dispersions of spherical carbides in a ferrite matrix. The chapter concludes with a brief discussion on the mechanical properties of ferrite/pearlite microstructures in medium-carbon steels.
You do not currently have access to this chapter.
Citation
Normalizing, Annealing, and Spheroidizing Treatments; Ferrite/Pearlite and Spherical Carbides, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 277–291, https://doi.org/10.31399/asm.tb.spsp2.t54410277
Download citation file:
Related Book Content
Pearlite, Ferrite, and Cementite
Steels: Processing, Structure, and Performance (Second Edition)
Equilibrium Phases and Constituents in the Fe-C System
Metallography of Steels Interpretation of Structure and the Effects of Processing
Heat Treatment of Steel
Elements of Metallurgy and Engineering Alloys
Annealing of Steel
Steel Heat Treating Fundamentals and Processes
Annealing, Normalizing, Martempering, and Austempering
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Heat Treatment of Cast Irons
Practical Heat Treating Basic Principles
Microstructures, Processing, and Properties of Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Heat Treating of Steel
Metals Handbook Desk Edition (2nd Edition)
Low-Carbon Irons and Steels
Light Microscopy of Carbon Steels
Annealing of Metals and Normalizing of Steel
Practical Heat Treating Basic Principles