Chapter 5: Martensite
-
Published:2015
Page range:
63 - 97
The formation of martensite is characterized by its athermal transformation kinetics, crystallographic features, and development of fine structure. This chapter describes the diffusionless, shear-type transformation of austenite to martensite and how it affects the morphology and microstructure of heat-treatable carbon steels. It also provides information on lath and plate martensite and how they differ in structure and deformation properties.
You do not currently have access to this chapter.
Citation
Martensite, Steels: Processing, Structure, and Performance, 2nd ed., By George Krauss, ASM International, 2015, p 63–97, https://doi.org/10.31399/asm.tb.spsp2.t54410063
Download citation file:
Related Book Content
Models for Martensitic Transformations
Fundamentals of Modeling for Metals Processing
Martensitic Structures
Metallography and Microstructures
Tempering of Martensite
Light Microscopy of Carbon Steels
Introduction to Phase Transformations
Elements of Metallurgy and Engineering Alloys
Hardness and Hardenability
Steels: Processing, Structure, and Performance (Second Edition)
Quenching of Titanium and Control of Residual Stresses
Heat Treating of Nonferrous Alloys
Microstructures and Properties of Carburized Steels
Heat Treating of Irons and Steels
Fundamentals of Steel Heat Treatment
Practical Heat Treating Basic Principles
Fracture of a Rail Arising From Flame-Cutting
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Transformation of Austenite
Light Microscopy of Carbon Steels