Skip Nav Destination
ASM Technical Books
Steels: Processing, Structure, and Performance (Second Edition)Available to Purchase
ASM International
ISBN electronic:
978-1-62708-265-5
Publication date:
2015
Steels: Processing, Structure, and Performance, Second Edition describes the physical metallurgy of steels. The book contains information on processing, alloying, microstructure, deformation, and fracture as well as hardenability, tempering, residual stress, surface engineering, and embrittlement. It discusses the properties of various types of steel, including low-carbon sheet steels, pearlitic rail and wire steels, quench and tempered medium- and high-carbon martensitic steels as well as stainless steels and tool steels. For information on the print version, ISBN 978-0-87170-641-6, follow this link.
Steels: Processing, Structure, and Performance
By: George Krauss
https://doi.org/10.31399/asm.tb.spsp2.9781627082655
ISBN (electronic): 978-1-62708-265-5
Publisher: ASM International
Published: 2015
Download citation file: