Properties and Selection of Aluminum Alloys
Fatigue of Aluminum Alloys[1]
-
Published:2019
Abstract
This article describes the effects of cyclic fatigue properties on aluminum alloys. It provides a discussion on strain-control fatigue and the effects of two microstructural features on the strain life of aluminum alloys: shearable precipitates and precipitate-free zones. The article discusses various models of fatigue crack growth (FCG) and the effects of alloy microstructure and composition on FCG.
J. Gilbert Kaufman, Fatigue of Aluminum Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 52–78, https://doi.org/10.31399/asm.hb.v02b.a0006549