Abstract
The development of aluminum alloys has progressed along two tracks: heat treatable and non-heat treatable. The Aluminum Association alloy composition limits and product temper are defined for major alloying elements. This article summarizes the historical evolution of the different series of wrought aluminum alloys (1xxx to 8xxx) and discusses their applications based on the alloying system introduced by the Aluminum Association.
You do not currently have access to this chapter.
Citation
Robert Sanders, James Staley, A History of Wrought Aluminum Alloys and Applications, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 157–201, https://doi.org/10.31399/asm.hb.v02b.a0006516
Download citation file:
Related Book Content
Heat Treating of Alloy Steels
Practical Heat Treating (Second Edition)
Aluminum and Aluminum Alloys
Alloying Understanding the Basics
Tool Steels and High-Speed Steels
Metallurgy for the Non-Metallurgist (Second Edition)
Alloys and Heat Treatment Choices
Aluminum Castings Engineering Guide
Physical Metallurgy of Aluminum Alloys
Aluminum Science and Technology
Hardenable Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Friction and Wear of Aluminum Alloys and Composites
Friction, Lubrication, and Wear Technology
Nominal Compositions and Composition Limits for Wrought Aluminum Alloys
Properties and Selection of Aluminum Alloys
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Tribological Properties of Copper Alloys
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications