6061 and Alclad 6061: General Structural Alloy
-
Published:2019
Abstract
The general structural alloy 6061 is a balanced alloy containing silicon and magnesium in appropriate proportions to form magnesium silicide, which makes the alloy precipitation hardenable. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 6xxx series alloy.
You do not currently have access to this chapter.
Citation
6061 and Alclad 6061: General Structural Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 388–393, https://doi.org/10.31399/asm.hb.v02b.a0006716
Download citation file:
Related Book Content
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
5083 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys
6463 Bright-Finishing Extrusion Alloy
Properties and Selection of Aluminum Alloys