7475: Controlled-Toughness Sheet and Plate Alloy
-
Published:2019
Abstract
Alloy 7475 is a controlled-toughness alloy for sheet and plate product forms. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 7xxx series alloy.
You do not currently have access to this chapter.
Citation
7475: Controlled-Toughness Sheet and Plate Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 457–461, https://doi.org/10.31399/asm.hb.v02b.a0006747
Download citation file:
Related Book Content
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
7175 and 7475 High-Purity Versions of 7075
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys
6061 and Alclad 6061 General Structural Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys