Properties and Selection of Aluminum Alloys
2xxx Aluminum Alloy Datasheets
-
Published:2019
Abstract
This article illustrates the relationships among commonly used 2xxx series alloys. It contains tables that list values for composition limits of aluminum-lithium alloys, and aerospace alloys and their temper conditions according to primary design requirements.
2xxx Aluminum Alloy Datasheets, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 287–289, https://doi.org/10.31399/asm.hb.v02b.a0006594