Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of Al-3.5Mg alloys 5154 and 5154A.
You do not currently have access to this chapter.
Citation
5154 and 5154A: Al-3.5Mg Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 360–361, https://doi.org/10.31399/asm.hb.v02b.a0006699
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
535.0, A535.0, and B535.0 Al-Mg High-Strength Casting Alloy
Properties and Selection of Aluminum Alloys
511.0, 512.0 and 513.0 Al-Mg Moderate-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys
6061 and Alclad 6061 General Structural Alloy
Properties and Selection of Aluminum Alloys