6013: High-Strength Al-Mg-Si-Cu Alloy
-
Published:2019
Abstract
Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy, developed for extruded automotive bumpers. This datasheet provides information on key alloy metallurgy, processing effects on physical, tensile, static and fracture properties, and fabrication characteristics of this 6xxx series alloy.
You do not currently have access to this chapter.
Citation
6013: High-Strength Al-Mg-Si-Cu Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 379–381, https://doi.org/10.31399/asm.hb.v02b.a0006711
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
6151 Aluminum Forging Alloy
Properties and Selection of Aluminum Alloys
5182 Sheet Alloy
Properties and Selection of Aluminum Alloys
332.0 Al-Si-Cu Permanent-Mold Casting Alloy
Properties and Selection of Aluminum Alloys
5086 and Alclad 5086 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys
7055 High-Strength Plate and Extrusion Alloy
Properties and Selection of Aluminum Alloys
Fatigue and Fracture Properties of Aluminum Alloy Castings
Fatigue and Fracture
6069 High-Strength Extrusion Alloy
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys