Properties and Selection of Aluminum Alloys
2040: High-Temperature Strength Alloy
-
Published:2019
Abstract
Alloy 2040 is a forging alloy with a significant improvement in elevated temperature properties over alloys 2014 and 2219. This datasheet provides information on composition limits of 2040 and provides a comparison of design mechanical properties of 2040 and 2014.
2040: High-Temperature Strength Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 308, https://doi.org/10.31399/asm.hb.v02b.a0006602