Skip Nav Destination
ASM Handbook
Properties and Selection of Aluminum Alloys
Edited by
ASM International
Volume
2B
ISBN electronic:
978-1-62708-210-5
Publication date:
2019
Book Chapter
7072: Cladding and Fin Stock
-
Published:2019
Abstract
This datasheet provides information on composition limits, ASTM product specifications, processing effects on physical and mechanical properties, and applications of cladding fin stock 7072.
You do not currently have access to this chapter.
Citation
7072: Cladding and Fin Stock, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 431, https://doi.org/10.31399/asm.hb.v02b.a0006736
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.
Related Book Content
7076 High-Strength Forging Alloy
Properties and Selection of Aluminum Alloys
2040 High-Temperature Strength Alloy
Properties and Selection of Aluminum Alloys
7349 Extrusion Alloy
Properties and Selection of Aluminum Alloys
2297 and 2397 Plate for Fatigue Critical Applications
Properties and Selection of Aluminum Alloys
Mechanical Properties and Testing of Titanium Alloys
Titanium Physical Metallurgy, Processing, and Applications
2524 Tough Moderate-Strength Sheet and Thin Plate
Properties and Selection of Aluminum Alloys
2196 and 2296 Aerospace Extrusion Alloy
Properties and Selection of Aluminum Alloys
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Tribological Properties of Copper Alloys
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
1 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys