Properties and Selection of Aluminum Alloys
711.0 and 712.0: Natural Aging Casting Alloys
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and applications of natural aging casting alloys 711.0 and 712.0. The fatigue strength of smooth and notched permanent mold aluminum casting of C712.0-F is illustrated.
Sign in
ASM members
Member Sign In711.0 and 712.0: Natural Aging Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 587–588, https://doi.org/10.31399/asm.hb.v02b.a0006587