710.0: Sand-Casting Alloy
-
Published:2019
Abstract
Alloy 710.0 is a natural-aging aluminum alloy produced by sand casting and suitable for highly stressed castings. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 7xxx series alloy.
710.0: Sand-Casting Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 585–586, https://doi.org/10.31399/asm.hb.v02b.a0006586