535.0, A535.0, and B535.0: Al-Mg High-Strength Casting Alloy
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of Al-Mg high-strength casting alloy 535.0.
You do not currently have access to this chapter.
Citation
535.0, A535.0, and B535.0: Al-Mg High-Strength Casting Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 583–584, https://doi.org/10.31399/asm.hb.v02b.a0006585
Download citation file:
Related Book Content
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
357.0 and Variations A357.0 to F357.0 Al-Si-Mg High-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5154 and 5154A Al-3.5Mg Alloy
Properties and Selection of Aluminum Alloys
511.0, 512.0 and 513.0 Al-Mg Moderate-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
356.0 and A356.0 Al-Si-Mg High-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys