Abstract
This article is a compilation of tables that present information on austenitizing temperatures for direct-hardening carbon and alloy steels, case depth of steels for different carburizing times and temperatures, typical heat treatments for case hardening of carbon and carburizing of alloy steels, as well as direct hardening of carbon steels and alloy steels.
You do not currently have access to this chapter.
Citation
Austenitizing and Typical Heat Treatment Temperatures for Steels, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 545–549, https://doi.org/10.31399/asm.hb.v04d.a0005996
Download citation file:
Related Book Content
Introduction to Heat Treating of Tool Steels
Heat Treating of Irons and Steels
Steel Heat Treating Process Control—An Introduction
Steel Heat Treating Technologies
Basics of Distortion and Stress Generation during Heat Treatment
Steel Heat Treating Technologies
Austenitizing in Steels
Steel Heat Treating Fundamentals and Processes
Selection of Carburizing Steels
Heat Treating of Irons and Steels
Introduction to Cast Iron Heat Treatment
Cast Iron Science and Technology
Heat Treating of High-Speed Tool Steels
Heat Treating of Irons and Steels
Steel Selection for Hardening
Heat Treating of Irons and Steels
Martempering of Steels
Steel Heat Treating Fundamentals and Processes
Temperature Measurement
Steel Metallurgy for the Non-Metallurgist