Skip Nav Destination
ASM Handbook
Heat Treating of Irons and Steels
Edited by
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4D
ISBN electronic:
978-1-62708-168-9
Publication date:
2014
Book Chapter
Steel Cross Reference to AISI/SAE Designations
-
Published:2014
Abstract
This article is a compilation of tables that present information on cross-referencing of steel designations that are followed in France, Germany, Italy, Japan, Sweden, and Britain to AISI/SAE.
Topics
Cast iron,
Steel,
Carbon steel,
High-alloy steel,
Low-alloy steel,
Tool steel,
Gears,
Heat treatment,
Boron,
Copper
You do not currently have access to this chapter.
Citation
Steel Cross Reference to AISI/SAE Designations, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 572–576, https://doi.org/10.31399/asm.hb.v04d.a0006000
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.
Related Book Content
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
History and Primary Steel Processing
Steels: Processing, Structure, and Performance (Second Edition)
Steel Hardness Conversions
Metallurgy for the Non-Metallurgist (Second Edition)
Introduction
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Decarburization of Steels
Practical Heat Treating (Second Edition)
Temper Colors for Steels
Failure Analysis of Heat Treated Steel Components