Distortion in Tool Steels[1]
-
Published:2014
Abstract
Distortion, encompassing all irreversible dimensional changes, is of two main types: size distortion and shape distortion. This article provides an overview of the nature and causes of distortion and discusses the process and material aspects of distortion specific to steels and tool steels. It also discusses the prediction of distortion and residual stresses by heat treatment simulation for optimizing production processes. The advantages and limitations of heat treatment simulation are also described.
Sign in
ASM members
Member Sign InReinhold Schneider, Rafael Mesquita, Wolfgang Schützenhöfer, Distortion in Tool Steels, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 300–311, https://doi.org/10.31399/asm.hb.v04d.a0005980
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.