Front End Loader Hoist Lift Hose Failure
-
Published:2019
Abstract
A hoist lift hose on a loader failed catastrophically. The hoses were a 100R13 type (as classified in AS3791-1991) with 50.8 mm nominal internal diameter. They consisted of six alternating spirals of heavy wire around a synthetic rubber inner tube with a synthetic rubber outer sheath. Failure of the lift hose was approximately 50 to 100 mm away from the "upper" end of the hose, with the straight coupling that attaches to the hydraulic system. The return hose was in much better condition, with no apparent deformation and only small areas of mechanical damage to the outer sheath. There...
Sign in
ASM members
Member Sign InS. Krismer, Front End Loader Hoist Lift Hose Failure, ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.conag.c9001635
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.