ASM Failure Analysis Case Histories: Processing Errors and Defects
ASM Failure Analysis Case Histories: Processing Errors and Defects documents more than 110 cases of structural and/or functional failure attributed to manufacturing defects associated with primary and secondary processes, including melting, casting, forging, forming, and heat treating. Cases also examine failures stemming from cleaning, finishing, coating, and plating defects, as well as failures due to machining, injection molding, welding, and brazing errors. The cases describe the investigation, identify the primary cause, and include remedial solutions. These case histories have been compiled from a wide variety of ASM International publication types, including ASM Handbook volumes, conference proceedings, technical books, journals, and magazines.
Download citation file:
Table of Contents
-
Brazing and Soldering Defects
-
Bulk Forming Defects
-
An Investigation of the Development of Defects During Flow Forming of High Strength Thin Wall Steel TubesByK.M. Rajan;K.M. RajanArmament Research and Development EstablishmentSearch for other works by this author on:K. NarasimhanK. NarasimhanDepartment of Metallurgical Engineering and Materials ScienceSearch for other works by this author on:
-
-
Casting Defects
-
Cracked Cast Iron CrankcasesByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Failure Analysis of an Aluminum CastingBySteven C. MedeirosSteven C. MedeirosAir Force Research LabSearch for other works by this author on:
-
Failure of Die Cast Aluminum Cluster Bomb Tailcone AssembliesByM. PepiM. PepiU.S. Army Research Laboratory, Weapons and Materials Research Directorate, AMSRL-WM-MDSearch for other works by this author on:
-
Metal Waves or Laking on Zinc-Based DiecastingsByGustav R. Perger;Gustav R. PergerCSIRO, Division of Tribophysics, University of MelbourneSearch for other works by this author on:Peter M. RobinsonPeter M. RobinsonCSIRO, Division of Tribophysics, University of MelbourneSearch for other works by this author on:
-
Metallic Inclusions in SteelByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Primary Grain Boundary Cracks in Cast Ingots and Flaky CrankshaftsByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Steel Casting with Insufficient Strength PropertiesByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Cleaning and Finishing Defects
-
Discoloration of a Stainless Steel Tube after PicklingByS.J. SuessS.J. SuessStork Techniment, Inc.Search for other works by this author on:
-
Coating and Plating Defects
-
Brittle Zinc Layer on a Hot-Galvanised HookByEgon KauczorEgon KauczorStaatliches Materialprüfungsamt an der FachhochschuleSearch for other works by this author on:
-
Fractures of Electro-Galvanized Cylinderhead ScrewsByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Hydrogen Induced Cracking of a Tappet Adjusting ScrewByB.V. KrishnaB.V. KrishnaMaterials Science & Technology Division, Thapar Centre for Industrial Research and Development Thapar Technology CampusSearch for other works by this author on:
-
Plating Adherence Problems in Electronic ComponentsByArun KumarArun KumarMetallurgical Services Scanning Electron Analysis Laboratories, Inc.[1]
Manager
Search for other works by this author on:
-
Forging Defects
-
Use of Electron Fractography to Diagnose Cracking in a 7075-T6 Aluminum ForgingByJames A. ScottJames A. ScottGroup Leader, Engineering, Metallurgical Engineering Requirements, Aircraft Div., McDonnell Douglas Corp.Search for other works by this author on:
-
Heat Treating Defects
-
Brittleness in Copper and Copper Alloys With Particular Reference to Hydrogen EmbrittlementByA. Matting;A. MattingInstitut A für Werkstoffkunde der Technischen Hochschule Hannover
Prof.
Search for other works by this author on:Ruth ZieglerRuth ZieglerInstitut A für Werkstoffkunde der Technischen Hochschule HannoverSearch for other works by this author on: -
Cracks in Flame Hardened Operation HandlesByEgon KauczorEgon KauczorWerkstoffprüfamt der Freien und HansestadtSearch for other works by this author on:
-
DecarburizationByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Investigation of a Case Hardened SleeveByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Investigation of Cracking and Erratic Behavior of the Uranium-Titanium AlloyByE. L. BirdE. L. BirdMaterials Engineering Department, Development Division, Oak Ridge Y-12 PlantSearch for other works by this author on:
-
Poorly Drawable Steel Wire for Ball BearingsByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Steel Hardenability and Failure AnalysisByBrett A. MillerBrett A. MillerStork Technimet, Inc.Search for other works by this author on:
-
Injection Molding Defects
-
Machining Defects
-
Stress Cracks in Brass Pipe CouplingsByKarin KuhnKarin KuhnMax-Planck-Institut für Metallforschung, Institut für SondermetalleSearch for other works by this author on:
-
Metal Production Defects
-
An Example of Decarburization in Alloy Steels and Its Effect on Further ProcessingByP. K. ChatterjeeP. K. ChatterjeeMinistry of Defense, Controllerate of Inspection (Metals)Search for other works by this author on:
-
Analysis of Center Burst During Hot ForgingByB. Vamsi Krishna;B. Vamsi KrishnaMaterials Science & Technology Division, Thapar Centre for Industrial Research and Development, Thapar Technology CampusSearch for other works by this author on:R.K. SidhuR.K. SidhuMaterials Science & Technology Division, Thapar Centre for Industrial Research and Development, Thapar Technology CampusSearch for other works by this author on:
-
Cast Ingot Cracked During ForgingByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Cast Steel Housing with Grain Boundary PrecipitatesByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
-
Sheet Forming Defects
-
Boiler Tube Cracked During BendingByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Broken Slide of a Friction PressByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Cracked Pipe Elbow of a Hydraulic InstallationByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Improper Fabrication Rotating Blades Results in Premature FailureByFred W. TatarFred W. TatarFactory Mutual Research CorporationSearch for other works by this author on:
-
-
Welding Defects
-
Analysis of Porosity Associated with Hanford 3013 Outer Container WeldsByW.L. Daugherty;W.L. DaughertyWestinghouse Savannah River CompanySearch for other works by this author on:G.R. CannellG.R. CannellFluor Federal ServicesSearch for other works by this author on:
-
Broken-Off Bearing Bosses of Scrap ShearsByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Cracking of Pipe Nipples in WeldingByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Leaky Socket Pipe from the Safety Return Circuit of a Heating InstallationByEgon KauczorEgon KauczorStaatliches Materialprüfungsamt an der FachhochschuleSearch for other works by this author on:
-
On-Site Nondestructive Metallographic Examination of MaterialsByJohn W. SimmonsJohn W. SimmonsLockheed Missiles and Space Co., Inc.Search for other works by this author on:
-
Plug Weld Defects in Low-Carbon Steel Bomb FinsByM. PepiM. PepiU.S. Army Research Laboratory, Weapons and Materials Research Directorate, AMSRL-WM-MDSearch for other works by this author on:
-
Steel Socket Pipe Conduit Cracked Next to Weld SeamByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
Welded Pipes with Hard SpotsByFriedrich Karl Naumann;Friedrich Karl NaumannMax-Planck-Institut für EisenforschungSearch for other works by this author on:Ferdinand SpiesFerdinand SpiesMax-Planck-Institut für EisenforschungSearch for other works by this author on:
-
-
Welding Defects