Book Chapter
Damage of a Screw in the Seal Coupling
By
B. Kosec
;
B. Kosec
University of Ljubljana, NTF—Department of Materials and Metallurgy
Search for other works by this author on:
L. Kosec
;
L. Kosec
University of Ljubljana, NTF—Department of Materials and Metallurgy
Search for other works by this author on:
P. Skraba
;
P. Skraba
University of Ljubljana, NTF—Department of Materials and Metallurgy
Search for other works by this author on:
F. Bizjan
F. Bizjan
University of Ljubljana, Faculty of Mechanical Engineering
Search for other works by this author on:
-
Published:2019
Abstract
The damage to a screw on the head of a 1.8 liter personal car engine was nucleated as the result of common disadvantageous environmental influences and reversed loads leading to corrosion fatigue.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
B. Kosec, L. Kosec, P. Skraba, F. Bizjan, Damage of a Screw in the Seal Coupling, ASM Failure Analysis Case Histories: Mechanical and Machine Components, ASM International, 2019, https://doi.org/10.31399/asm.fach.mech.c9001614
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.
Related Book Content
Corrosion Fatigue Cracking of Wire Ropes
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Fatigue Failure of Crane Clevis Bracket
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Copper Alloys: Atlas of Fractographs
Fractography
Metallurgical Failure Analysis of a Broken Compression Hip Screw Surgical Implant
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Turbine Blade Failures, Who Pays?
ASM Failure Analysis Case Histories: Power Generating Equipment
Tower Crane Failure
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Failure of a Service Water Pump Shaft
Handbook of Case Histories in Failure Analysis
Fatigue Fracture of a Helicopter Tail Rotor Blade Due to Field-Induced Corrosion
Handbook of Case Histories in Failure Analysis
Failure Analysis of a Cracked Low-Pressure Turbine Blade
Handbook of Case Histories in Failure Analysis
Cause and Prevention of Fatigue Failures in Boiler Tubing
ASM Failure Analysis Case Histories: Power Generating Equipment