ASM Failure Analysis Case Histories: Chemical Processing Equipment
The Failure of Titanium Clad Tube Sheet in Heat Exchanger by Fatigue Cracking and Corrosion
-
Published:2019
Abstract
Corrosion failure occurred in a titanium clad tubesheet because of a corrosive tube-side gas-liquid mixture leaking through fatigue cracks in the seal welds at tube-to-tubesheet joints. The tubesheet was a carbon steel plate clad with titanium on the tube side face. The seal weld cracks were initiated by cyclic stress imposed by exchanger tubes. The gas-liquid mixture passed through cracks under tube-side pressure, resulting in severe corrosion of the steel backing plate. The failure started with the loosening of the expanded tube-to-tubesheet joints. Loose joints allowed the exchanger tubes to impose load on seal welds and the shell side...
Sign in
ASM members
Member Sign InC. H. Hsu, The Failure of Titanium Clad Tube Sheet in Heat Exchanger by Fatigue Cracking and Corrosion, ASM Failure Analysis Case Histories: Chemical Processing Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.chem.c9001570
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.