Burning of Chlorine Compressor Piston Rods
-
Published:2019
Abstract
Initially, two vertical double-acting two-stage compressors delivering chlorine gas at a pressure of 100 psi appeared to be running satisfactorily. About six months later the LP piston-rod of the No. 2 compressor failed due to burning, the compressor being worked double-acting at the time. About five months later, the HP piston rod of the No. 1 compressor failed in a similar manner. Specimens for microscopic examination were cut from the rod in the region of the failure and from the extreme end that had been situated above the piston and hence not subjected to an appreciable rise in temperature....
Sign in
ASM members
Member Sign InBurning of Chlorine Compressor Piston Rods, ASM Failure Analysis Case Histories: Chemical Processing Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.chem.c9001408
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.