Abstract
A 60.3 mm (2.375 in.) diam drive shaft in the drive train of an overhead crane failed. The part submitted for examination was a principal drive shaft that fractured near a 90 deg fillet where the shaft had been machined down to 34.9 mm (1.375 in.) to serve as a wheel hub. A 9.5 mm (0.375 in.) wide x 3.2 mm (0.125 in.) deep keyway was machined into the entire length of the hub, ending approximately 1.6 mm (0.062 in.) away from the 90 deg fillet. A second shaft was also found to have cracked at a change in...
Sign in
ASM members
Member Sign InFailure of an Overhead Crane Drive Shaft Due to Rotating-Bending Fatigue, ASM Failure Analysis Case Histories: Material Handling Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.matlhand.c0091092
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.